Hawk
Well-Known Member
So those are tin oxide swirls. This mold has made me jack the temp on my furnace up to levels I have never used before.
Got the furnace set to 700-710 Degrees.
I'm running the mold really hot and fast. Have to use a fan to cool the sprue plates. Bullets are frosted in the middle and bases, but not so much on the nose.
If I don't run this hot and fast, I get wrinkles in the nose.
I want my bullets to look like Ben's. Bright and shiny
Got the furnace set to 700-710 Degrees.
I'm running the mold really hot and fast. Have to use a fan to cool the sprue plates. Bullets are frosted in the middle and bases, but not so much on the nose.
If I don't run this hot and fast, I get wrinkles in the nose.
I want my bullets to look like Ben's. Bright and shiny