Brother_Love
Well-Known Member
I need to do a batch of smelting. I have WW, dental xray lead, industrial counterweights and a small amount of range scrap. What is the ideal temp to keep all the elements together? I am fluxing with beeswax.
Thank you.
Unfortunately I have about 200 lbs someone gave me but I think it is contaminated with zinc. Is there a "home remedy or test" I can use to find out. I would not want to mix it with my other ally if it is tainted.
Thank you.
Unfortunately I have about 200 lbs someone gave me but I think it is contaminated with zinc. Is there a "home remedy or test" I can use to find out. I would not want to mix it with my other ally if it is tainted.